Inter-fibre failure of through-thickness reinforced laminates in combined transverse compression and shear load

dc.contributor.authorCui, Hao
dc.contributor.authorMelro, António R.
dc.contributor.authorYasaee, Mehdi
dc.date.accessioned2018-08-13T09:18:04Z
dc.date.available2018-08-13T09:18:04Z
dc.date.freetoread2019-05-29
dc.date.issued2018-06-13
dc.description.abstractExtensive studies have been reported on the improvement of through-thickness reinforcement to inter-laminar performance of composite laminates; current understanding on the in-plane performance is relatively limited, although it is also concerned in industrial application. The influence of through-thickness reinforcement (Z-pinning) on the inter-fibre failure in compression of unidirectional laminates was investigated. Both unpinned and Z-pinned laminates were tested at four different off-axis angles, representing different combinations of transverse compression and in-plane shear stress. It was found that the stiffness of Z-pinned laminates decreased significantly in all off-axis angles. The failure strain and strength were reduced in shear dominated failure modes, while improved in the compression dominated failure modes by the presence of the Z-pins. A further investigation on the angle of failure plane was carried out and a comparison with analytical failure models is presented.en_UK
dc.identifier.citationCui H, Yasaee M, Melro A, Inter-fibre failure of through-thickness reinforced laminates in combined transverse compression and shear load, Composites Science and Technology, Volume 165, Issue September 2018, pp. 48-57en_UK
dc.identifier.cris20627459
dc.identifier.issn0266-3538
dc.identifier.urihttp://dx.doi.org/10.1016/j.compscitech.2018.06.011
dc.identifier.urihttps://dspace.lib.cranfield.ac.uk/handle/1826/13393
dc.language.isoenen_UK
dc.publisherElsevieren_UK
dc.rightsAttribution-NonCommercial-NoDerivatives 4.0 International*
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.subjectZ-pinen_UK
dc.subjectInter-fibre failureen_UK
dc.subjectStrengthen_UK
dc.subjectFibre volume fractureen_UK
dc.titleInter-fibre failure of through-thickness reinforced laminates in combined transverse compression and shear loaden_UK
dc.typeArticleen_UK

Files

Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Inter-fibre_failure_of_through-thickness-2018.pdf
Size:
2.2 MB
Format:
Adobe Portable Document Format
Description:
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.63 KB
Format:
Item-specific license agreed upon to submission
Description: