Data: Cure kinetics, glass transition advancement and chemo-rheological modelling of an epoxy vitrimer based on disulphide metathesis: dataset

dc.contributor.authorIfeanyi Anagwu, Festus
dc.contributor.authorSkordos, Alex
dc.date.accessioned2024-06-07T03:30:40Z
dc.date.available2024-06-07T03:30:40Z
dc.date.issued2023-10-18 08:39
dc.description.abstractThe dataset consists of the results of cure kinetics, glass transition advancement, chemorheology and stress relaxation experiments for the DGEBA/4-APDS epoxy vitrimer. The heading of each column contains the quantity measured and the unit of measurement. The cure kinetics dataset (Cure-kinetics-dataset.xlsx) comprises time-temperature profiles and degrees of cure attained as well as the associated reaction rate data for 4 dynamic DSC experiments (1.25°C/min, 2.5°C/min, 5°C/min and 10°C/min) and 7 isothermal DSC experiments (140°C, 150°C, 160°C, 170°C, 180°C, 190°C and 200°C). Experimental results for each temperature and rate are presented in a separate spreadsheet. The chemorheology dataset (Chemorheology-dataset.xlsx) contains time, temperature and viscosity profile for 5 isothermal experiments (80°C, 90°C, 100°C, 110°C and 120°C). Experimental results for each temperature are presented in a separate spreadsheet. The stress relaxation dataset (Stress-relaxation-dataset.xlsx) contains decay time, temperature, stress, strain and relaxation modulus obtained in 5 isothermal experiments (180°C, 190°C, 200°C, 210°C and 220°C). Each spreadsheet represents an experiment at a particular temperature. The Tg advancement dataset (Tg-advancement-dataset.xlsx) contains time, temperature and heat flow profiles for 18 experiments carried out on partially cured samples. The data are organised in spreadsheets per DSC test; the thermal profile prior to the experiments is as follows: - Tg_1.25°C-min-220°C: DSC of uncured resin. - Tg_1.25°C-min-130°C: DSC of resin partially cured at 1.25°C/min from -50°C to 130°C. - Tg_1.25°C-min-136°C: DSC of resin partially cured at 1.25°C/min from -50°C to 136°C. - Tg_1.25°C-min-140°C: DSC of resin partially cured at 1.25°C/min from -50°C to 140°C. - Tg_1.25°C-min-145°C: DSC of resin partially cured at 1.25°C/min from -50°C to 145°C. - Tg_1.25°C-min-150°C: DSC of resin partially cured at 1.25°C/min from -50°C to 150°C. - Tg_1.25°C-min-160°C: DSC of resin partially cured at 1.25°C/min from -50°C to 160°C. - Tg_1.25°C-min-170°C: DSC of resin partially cured at 1.25°C/min from -50°C to 170°C. - Tg_1.25°C-min-180°C: DSC of resin partially cured at 1.25°C/min from -50°C to 180°C. - Tg_1.25°C-min-190°C: DSC of resin partially cured at 1.25°C/min from -50°C to 190°C. - Tg_2.5°C-min-170°C: DSC of resin partially cured at 2.5°C/min from -50°C to 170°C. - Tg_5°C-min-170°C: DSC of resin partially cured at 5°C/min from -50°C to 170°C. - Tg_10°C-min-170°C: DSC of resin partially cured at 10°C/min from -50°C to 170°C. - Tg_iso10min_150°C: DSC of resin partially cured isothermally at 150°C for 10 minutes. - Tg_iso20min_150°C: DSC of resin partially cured isothermally at 150°C for 20 minutes. - Tg_iso30min_150°C: DSC of resin partially cured isothermally at 150°C for 30 minutes. - Tg_iso40min_150°C: DSC of resin partially cured isothermally at 150°C for 40 minutes. - Tg_iso100min_150°C: DSC of resin partially cured isothermally at 150°C for 100 minutes (fully cured).
dc.description.sponsorshipTertiary Education Trust Fund [grant number TETF/ES/POLY/IMO STATE/TSAS/2019/VOL.I]
dc.identifier.citationAnagwu, Festus Ifeanyi; Skordos, Alex (2023). Data: Cure kinetics, glass transition advancement and chemo-rheological modelling of an epoxy vitrimer based on disulphide metathesis: dataset. Cranfield Online Research Data (CORD). Dataset. https://doi.org/10.17862/cranfield.rd.22890563
dc.identifier.doi10.17862/cranfield.rd.22890563
dc.identifier.urihttps://dspace.lib.cranfield.ac.uk/handle/1826/22017
dc.publisherCranfield University
dc.relation.isreferencedbyhttps://doi.org/10.1016/j.polymer.2023.126427'
dc.rightsCC BY 4.0
dc.rights.urihttps://creativecommons.org/licenses/by/4.0/
dc.subject'Cure kinetics'
dc.subject'vitrimers'
dc.subject'composites'
dc.subject'chemo-rheology'
dc.subject'glass transition'
dc.subject'topology transition'
dc.titleData: Cure kinetics, glass transition advancement and chemo-rheological modelling of an epoxy vitrimer based on disulphide metathesis: dataset
dc.typeDataset

Files

Original bundle
Now showing 1 - 4 of 4
No Thumbnail Available
Name:
Tg-advancement-dataset.xlsx
Size:
10.05 MB
Format:
Microsoft Excel XML
No Thumbnail Available
Name:
Cure-kinetics-dataset.xlsx
Size:
145.8 KB
Format:
Microsoft Excel XML
No Thumbnail Available
Name:
Chemorheology-dataset.xlsx
Size:
80.89 KB
Format:
Microsoft Excel XML
No Thumbnail Available
Name:
Stress-relaxation-dataset.xlsx
Size:
27.25 KB
Format:
Microsoft Excel XML