dc.description.abstractIn this paper, electrohydrodynamic atomization combined with a polymeric micromoulding technique was used to form PZT single element devices using a PZT sol-gel slurry without an etching process. The PZT single element device was initially designed to work as a piezoelectric ultrasonic transducer consisting of a circular or a square of various sizes, which wasproduced and used to evaluate the process. The resulting PZT device had a homogenous microstructure. It was observed that the relative permittivity of the circular and square single element devices was especially high at small size due to the fringe effect. The results show that the radius and width of the PZT single circular and square element devices with a thickness of 15μm should be bigger than 400μm in order to reduce the fringe effecen_UK
dc.identifier.citationD. Z. Wang and R. A. Dorey, Formation of PZT thick film single elements using EDHA deposition. Materials Science Forum, 2009, Vol. 628-629, pp405-410.
dc.identifier.issn0255-5476-
dc.identifier.urihttp://dx.doi.org/10.4028/www.scientific.net/MSF.628-629.405-
dc.identifier.urihttp://dspace.lib.cranfield.ac.uk/handle/1826/6196
dc.publisherTranstec Publications; 1999en_UK
dc.titleFormation of PZT thick film single elements using EDHA depositionen_UK
dc.typeArticle-

Files

Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Formation_of_PZT-2009.pdf
Size:
614.69 KB
Format:
Adobe Portable Document Format
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
18 B
Format:
Plain Text
Description: