dc.description.abstract | A novel method for the densification of sol-gel films is presented. After elimination of organic decomposition products by heat-treatment at 350 °C and 450 °C, the films are isopressed prior to crystallisation at 550 °C. Consequently, porous lead zirconate titanate films, ~0.7 um in thickness with pore sizes of ~0.1 um could be transformed into dense 0.2 um fil | en_UK |
dc.identifier.citation | Mikael A. Khan, Rajnish Kurchania, Silvana Corkovic, et al., Densification of lead zirconate titanate sol-gel coatings. Materials Letters, Volume 60, Issue 12, June 2006, Pages 1463-1465. | |
dc.identifier.issn | 0167-577X | - |
dc.identifier.uri | http://dx.doi.org/10.1016/j.matlet.2005.11.046 | - |
dc.identifier.uri | http://dspace.lib.cranfield.ac.uk/handle/1826/5208 | |
dc.language.iso | en_UK | en_UK |
dc.publisher | Elsevier Science B.V., Amsterdam. | en_UK |
dc.title | Densification of lead zirconate titanate sol-gel coatings | en_UK |
dc.type | Article | en_UK |