Mechanical performance and microstructural characterisation of titanium alloy-alloy composites built by wire-arc additive manufacture

Show simple item record

dc.contributor.author Davis, Alec E.
dc.contributor.author Breheny, Cameron I.
dc.contributor.author Fellowes, Jonathan W.
dc.contributor.author Nwankpa, U.
dc.contributor.author Martina, Filomeno
dc.contributor.author Ding, Jialuo
dc.contributor.author Machry, Thays
dc.contributor.author Prangnell, Phil
dc.date.accessioned 2019-09-23T15:33:26Z
dc.date.available 2019-09-23T15:33:26Z
dc.date.issued 2019-08-14
dc.identifier.citation Davis A, Breheny C, Fellowes J, et al., Mechanical performance and microstructural characterisation of titanium alloy-alloy composites built by wire-arc additive manufacture. Materials Science and Engineering: A, Volume 765, September 2019, Article number 138289 en_UK
dc.identifier.issn 0921-5093
dc.identifier.uri https://doi.org/10.1016/j.msea.2019.138289
dc.identifier.uri https://dspace.lib.cranfield.ac.uk/handle/1826/14555
dc.description.abstract A first stage study has been performed to investigate the potential for exploiting high deposition rate WAAM to print dual-alloy microstructures. Samples were built using alternating feed wires of commercially-pure Ti and Ti–6Al–4V. A high level of dilution occurred during deposition accompanied by effective liquid-phase mixing, producing a regular distribution of solidified melt tracks of approximate bimodal composition each less extreme than that of their respective constituent feed wires. The yield strength of the dual alloy composite material was approximately midway between that of the two alloys from which it was produced and exhibited a double inflection yield behaviour. Overall, because of the relatively coarse length scale there was not a significant property advantage in tensile loading above that of a chemically homogenous material, thus the main advantage of printing alternate alloys at this length scale is likely to reside more with increasing crack path tortuosity during fracture or fatigue loading. Importantly, the deposited material was found to have a refined β-grain structure suggesting that the composition gradients introduced by dual-alloy printing can disrupt the epitaxial columnar growth normally seen in WAAM deposits. en_UK
dc.language.iso en en_UK
dc.publisher Elsevier en_UK
dc.rights Attribution 4.0 International *
dc.rights.uri http://creativecommons.org/licenses/by/4.0/ *
dc.subject Titanium alloys en_UK
dc.subject Additive manufacturing en_UK
dc.subject Characterization en_UK
dc.subject Grains and interfaces en_UK
dc.subject Mechanical properties en_UK
dc.subject Fracture behaviour en_UK
dc.title Mechanical performance and microstructural characterisation of titanium alloy-alloy composites built by wire-arc additive manufacture en_UK
dc.type Article en_UK


Files in this item

The following license files are associated with this item:

This item appears in the following Collection(s)

Show simple item record

Attribution 4.0 International Except where otherwise noted, this item's license is described as Attribution 4.0 International

Search CERES


Browse

My Account

Statistics