Wray, Lesley-Anne; Ayre, David; Irving, Phil E.; Jackson, Paul A.; Jones, P. R.; Zhao, F.
(Elsevier, 2018-12-31)
Welded steel T-sections of different weld fillet geometries coated with water ballast tank protective coatings were subjected to thermal cycling with a temperature range from 60°C to -10°C. Cracks developed in the coatings ...